1.4044.5 / X22CrNi17

1.4044.5 / X22CrNi17

Round Bars 6–80 mm

Conforms with

Material properties: Tensile Strength 800–950 MPa, Yield Strength – MPa, Working temperature – °C

Equivalent or similar: SAE 51431

WL 1.4044 WL 1.4044, DIN EN 3506, UNS S43100, AISI 431C

WL 1.4044  is a stainless steel containing about 16% chromium with additions of nickel and achieves high mechanical properties through a conventional arc melting process. Due to moderate corrosion resistance, SAE 51431 is used in areas with lower corrosive requirements but higher mechanical properties than those of 410 stainless steel.

 

C: 0,12 – 0,20 %
Cr: 15,0 – 18,0 %
Mn: max. 1,0 %
Ni: 2,0 – 3,0 %
P: max. 0,035 %
S: 0,025 %
Si: max. 1,0 %